cemotech,ultraplast,stargel,cemo logo,celotech
cemotech,ultraplast,stargel,cemo logo,celotech
construction chemicals,cellulose ethers,starch ether,prestar,stargel,ultraplast
  • Home
  • Products 
    • Overview
    • Redispersible Powder
    • Superplasticizers
    • Powder Defoamer
    • Gypsum Retarder
    • Calcium Formate
    • Water repellent Agent
    • Modified Starch
  • Cemotech
  • News
  • Contact
  • …  
    • Home
    • Products 
      • Overview
      • Redispersible Powder
      • Superplasticizers
      • Powder Defoamer
      • Gypsum Retarder
      • Calcium Formate
      • Water repellent Agent
      • Modified Starch
    • Cemotech
    • News
    • Contact
Email
cemotech,ultraplast,stargel,cemo logo,celotech
cemotech,ultraplast,stargel,cemo logo,celotech
construction chemicals,cellulose ethers,starch ether,prestar,stargel,ultraplast
  • Home
  • Products 
    • Overview
    • Redispersible Powder
    • Superplasticizers
    • Powder Defoamer
    • Gypsum Retarder
    • Calcium Formate
    • Water repellent Agent
    • Modified Starch
  • Cemotech
  • News
  • Contact
  • …  
    • Home
    • Products 
      • Overview
      • Redispersible Powder
      • Superplasticizers
      • Powder Defoamer
      • Gypsum Retarder
      • Calcium Formate
      • Water repellent Agent
      • Modified Starch
    • Cemotech
    • News
    • Contact
Email
cemotech,ultraplast,stargel,cemo logo,celotech

What is the minimum film-forming temperature (MFT) of redispersible polymer powders?

· RDP,Vinabond

The minimum film-forming temperature refers to the minimum temperature at which polymers form a continuous film, expressed by MFT. If the cement hydration temperature is below this value, the energy supplied will not be enough to start film formation. At this time polymers will be present in the form of intermittent particles in the cement mortar. Only when the cement hydration temperature is higher than MFT of polymers can polymers form a uniform film structure and be distributed between cement hydration products, playing a bridging role when there is stress, effectively absorbing and transferring energy, thereby inhibiting the formation and development of cracks. Therefore, make sure that the MFT should be lower than the curing temperature of mortar in order to make redispersible polymer powders form a film in the hardened mortar.

broken image

ABOUT CEMOTECH

→ Suzhou Cemo New Material Technology Co.,Ltd is a high-tech enterprise specialized in construction additives.

→ Estabilished in 2011 and expanded production scale in 2015.

→ Our production capacity is 10,000 tons of redispersible polymer powder, 5000 tons of polycarboxylic acid superplasticizer, 3000 tons of melamine superplasticizer, 2000 tons of defoamer, gypsum retarder, hydrophobic agent and other additives.

Subscribe
Previous
What is the glass-transition temperature (Tg) of...
Next
The variety of Redispersible Polymer powders
 Return to site
Cookie Use
We use cookies to improve browsing experience, security, and data collection. By accepting, you agree to the use of cookies for advertising and analytics. You can change your cookie settings at any time. Learn More
Accept all
Settings
Decline All
Cookie Settings
Necessary Cookies
These cookies enable core functionality such as security, network management, and accessibility. These cookies can’t be switched off.
Analytics Cookies
These cookies help us better understand how visitors interact with our website and help us discover errors.
Preferences Cookies
These cookies allow the website to remember choices you've made to provide enhanced functionality and personalization.
Save